Mill and Pave 50 mm (50 mm ACWC)
- Area to be
repaired is demarcated and confirmed at site with the Engineer
representative.
- The milling
work shall be done as mentioned in 2.3.A.
- Subsequently,
tack coat (or other surface coating as per scope of works) shall be
applied as per specifications.
- 50 mm thick
of ACWC is then laid and compacted.
- Compaction shall follow the rolling
pattern established during the trial lay.
- The laid
material is to be let to cure for minimum of 6 hours and during this
duration the lane is to be closed from traffic.